High Coat Technik

Resistance in the pencil test (ASTM 3363 and JIS 5400-8.4)4H

Resistance to solvents (acetone), carried out using special constant pressure machine

6000 passages 

Resistance to rubbing, in which cloths were moistened with a normal household product, carried out using a special constant pressure machine

4000 passages
Gloss96 gloss
Resistance to salt spray mist(ASTMB 117 / UNI ISO 9227)> 1500  hours  
Adhesive strength (UNI 8574.6 /JIS 5400-8.5)10 (maximum evaluation points)


COMPARISON BETWEEB A NORMAL DIPPING VARNISH AND HIGH COAT

Scale of rising hardness values:

2B (-2), B (-1), HB (0), H (1), 2H (2), 3 H (3), 4H (4), 5H (5), ...

Note

The parts varnished with dipping varnish begin to corrode after 20 hours of being sprayed with a salt spray mist, while the articles treated with the HIGH COAT process show no signs of corrosion in the salt spray mist, even after 1500 hours.

NEWS!

We have recently obtained the general building inspectorate approval / general type approval (abz) for our clamp holders.

Take a look at our object assortement for architects.

The responsible use of resources is very important to us. That's why we try to recycle waste as best we can.

Easy and Versatile: Access Control via Voxio RFID Reader.

ESCAPE DOOR CONTROL THROUGH AN INTELLIGENT MODULAR SOLUTION....

Opening doors via Smartphone: ÜLock BLE and KleverKey can make it happen...

Südmetall has been carrying the "Leitbetrieb" seal since the turn of the year and thus sets a clear example of service quality. In the service desert...